Here is my version of how to produce your own heatbed with the toner transfer method:
Tips:
- I use 1200 or 1000 ppmm sandpaper to roughen the copper. This allows fine details.
- The laser printer is a cheap Samsung ML-2525W (69€).
- Watering of the ironed layout lasts just a few seconds, before the paper can be rubbed off with latex gloves on. The more toner is on the print, the longer you should water it before rubbing the layout off.
- The iron should be as hot as possible. The longer you iron the board, the less breaches in the layout will occur when removing the paper.
- Don't iron directly on the paper. Details will get smeared and lines will not be sharp. Use one or two layer of paper towel as a buffer between the iron and the layout.
- Use pressure but try to avoid to move the paper with the molten toner. It's a question of training to become perfect.
- Laminating instead of ironing seems more comfortable, but doesn't give the best quality possible.